Mr. Shashank, Can you give more details like what is the welding process, Pipe or Plate joint. In flow lines I use to see these type of indication in crude oil pipelines especially in 4" & 6". As per API 1104 I will reject due to size you mentioned. Regards, S.Senthilkumar
--- On Thu, 15/4/10, Shashank Vagal <nach_sam@yahoo.com> wrote:
From: Shashank Vagal <nach_sam@yahoo.com> Subject: [MW:4850] Radiographic film interpretation To: materials-welding@googlegroups.com Date: Thursday, 15 April, 2010, 8:16 PM
| Hi all, In one RT film we have a 10-12 mm spot with density 3.13. The weld density is 3.17 and the parent metal density is 3.3. It is apparently interpass LoF in the 2nd fill pass after hot pass (confirmed by UT, where the indication ht is approx 20%of DAC). Is there any or what is the criteria for acceptance/rejection based on density difference? Rgds, Shashank Vagal | -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
Send free SMS to your Friends on Mobile from your Yahoo! Messenger. Download Now! http://messenger.yahoo.com/download.php
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment