Hi Friend,
 
As per Ur below info,  refer ASME VIII Div I, UW-37 (f) miscellaneous welding requirements for ID stamping, just for Ur knowledge.
 
 
Normally we use welder traceability record, based on ASME QC Manual.
 
Cheers,
Sarav
 


 
On Fri, Jun 1, 2012 at 10:10 AM, RogerPhung <nvpUSA@msn.com> wrote:
 
To our Experts!
 
Please advise, where I can find in ASME Code for
the Welder ID and or FW ID:
MUST STAMP IT (stencil ID), but not using yellow or black
marker?
 
Thanks
 
RogerPhung
        
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Blog Archive